Q
EEA injection molded product ejector whitening
Q
Uneven color of EEA mixed with color masterbatch
A
Color masterbatch carrier matching and full dispersion are the key to color uniformity
Injection Molding EEA coloringcolor masterbatchcarrier compatibilitypigment dispersioncolor streaks
Q
Oil spots on EEA injection molded products
Q
Low weld line strength in EEA injection
Q
Insufficient EEA injection flow length ratio
A
Insufficient flow length ratio is caused by EEA high viscosity; high temperature, high pressure and large gate are the key
Injection Molding EEA injectionflow length ratiomelt viscosityinjection temperatureflow aid
Q
Severe EEA injection flash
A
Q
EEA injection warpage deformation
A
Warpage is caused by shrinkage difference and orientation stress; uniform mold temperature and holding are the key
Injection Molding EEA injectionwarpageshrinkage rateholding pressureannealing treatment
Q
EEA injection gate freezing too early
Q
EEA injection mold venting burnt
Q
EEA '2079851475616104452 demolding difficulty