EEA injection warpage deformation

Problembeschreibung
EEA injection molded products warped 2-3mm/100mm after demolding, flatness not up to standard
Ursachenanalyse
EEA shrinkage rate large and mold temperature uneven causing shrinkage difference in all directions; improper gate position, flow orientation stress unevenly released; insufficient cooling time
Lösung
1) Increase mold temperature to 40-60°C to reduce temperature difference; 2) Increase holding pressure to 50-70MPa; 3) Optimize gate position for uniform flow; 4) Extend cooling time; 5) Anneal to release residual stress
Wichtigste Erkenntnis
Warpage is caused by shrinkage difference and orientation stress; uniform mold temperature and holding are the key