Q
Oil spots on EEA injection molded products
Q
Low weld line strength in EEA injection
Q
Insufficient EEA injection flow length ratio
A
Insufficient flow length ratio is caused by EEA high viscosity; high temperature, high pressure and large gate are the key
Injection Molding EEA injectionflow length ratiomelt viscosityinjection temperatureflow aid
Q
Material sticking to the sizing sleeve of EEA extruded pipe
A
Sizing sleeve sticking is caused by elastomer adhesion characteristics; polishing and lubricating water are the key
Molding Process EEA pipesizing sleeve stickingpolishinglubricating waterelastomer adhesion
Q
Rough inner wall of EEA extruded pipe
Q
EEA extrusion film longitudinal streaks
Q
EEA film blocking, difficult delamination
Q
EEA extrusion profile bending deformation
A
Profile bending is caused by uneven cooling and uneven flow velocity; homogenization and alignment are the key to resolution
Extrusion & Post EEA extrusionbending deformationuniform coolinguniform flow velocitysizing sleeve
Q
Severe EEA injection flash
A
Q
Poor EEA extrusion film thickness uniformity
A
Film thickness uniformity requires coordinated optimization from three aspects: die design, gap adjustment and cooling
Extrusion & Post EEA filmthickness uniformitydie designextrusion swellair ring cooling