Product surface sagging
문제 현상
Flow marks or sagging appear on the product surface.
When this defect occurs in products of Process No.
2, it is usually related to a specific process parameter range or equipment status.
If it persists, it will directly affect the product qualification rate and production cycle, increasing material loss and rework costs.
Timely diagnosis and elimination is a basic requirement to ensure stable production.
원인 분석
1.
Process parameter factor: The material viscosity is too low, the injection speed is too fast, the mold temperature is high causing excessive flow, and the release agent is unevenly distributed.
2.
Mixing quality factor: In the RIM process, the mixing uniformity of the two components is the foundation of all quality; the Reynolds number of the mixing head, the impingement mixing energy, and the residence time distribution are the key engineering parameters that determine the mixing quality.
해결 방법
1.
Process parameter optimization and adjustment: Increase the material viscosity, reduce the injection speed, reduce the mold temperature, and apply the release agent evenly.
2.
Systematic troubleshooting method: RIM problem troubleshooting follows the order of "formulation -> mixing -> temperature control -> equipment".
First check the two-component ratio and catalyst dosage, then check the mixing head and self-cleaning function, next troubleshoot the raw material and mold temperature control, and finally check the accuracy of the metering pump and hydraulic system.
3.
Preventive management: Establish standardized process parameter cards and quality control limits for each mold/product, and regularly conduct process capability index (CPK) assessments.
For recurring problems, use fishbone diagrams or 5Why analysis to trace the root cause, and solidify countermeasures as PFMEA control points.
핵심 요약
This problem is a typical manifestation of product surface sagging in the RIM process, and the core of the solution lies in ensuring the precise ratio and sufficient mixing of the two components, while controlling the reaction temperature and curing conditions within the optimal window.
It is recommended to start troubleshooting from the mixing system and metering accuracy.