Separation of Spinning Oiling Agent in Freezing Weather

문제 현상
The spinning oiling agent or finishing agent adheres unevenly to the fiber, locally too much or too little, and the tow feels inconsistent. Uneven oiling agent directly affects the spinnability of the fiber—places with insufficient oiling have high friction and are prone to breakage, and places with excessive oiling have filaments sticking together and are not easy to separate into bundles. Uneven oiling agent distribution also causes inconsistent tension of the tow during drawing, leading to denier fluctuations and uneven drawing.
원인 분석
1. Spinning temperature factors: The spinning temperature determines melt viscosity and rheological behavior, directly affecting the spinnability, fineness uniformity, and surface quality of the fiber. Excessively high temperature leads to degradation yellowing and filament breakage; excessively low temperature leads to poor plasticization and increased extrusion pressure; it needs to be precisely set according to the chip IV value and stably controlled. 2. Cooling air field factors: The temperature, wind speed, and uniformity of side-blowing or circular-blowing air determine the solidification and forming quality of the fiber—too fast cooling leads to rough surface and increased internal stress, uneven cooling leads to inconsistent fineness among filaments in the same bundle, and low wind speed leads to filament sticking and filament breakage; air field parameters need to be precisely controlled.
해결 방법
1. Process parameter optimization and adjustment: Configure the storage tank with an oil agent temperature control system (above the phase separation temperature). 2. Systematic troubleshooting method: Troubleshooting of spinning problems follows the order of "chips → temperature → metering → spinneret → cooling air". First check the chip dryness and IV value, then verify the temperature of each section of the spinning manifold and piping, then verify the metering pump accuracy and pressure stability, further check the spinneret cleanliness and hole shape condition, and finally adjust the cooling air field parameters to make the wind speed and temperature evenly distributed. 3. Preventive management: Establish standardized process parameter cards and quality control limits for each mold/product, and regularly conduct process capability index (CPK) evaluations. For recurring problems, use fishbone diagrams or 5Why analysis to trace the root cause, and solidify countermeasures as PFMEA control points. Establish a regular equipment maintenance system and implement life management for key tooling such as dies/spinnerets/calender rolls/coating heads.
핵심 요약
This problem is a typical manifestation of separation of spinning oiling agent in freezing weather in melt spinning. The core of the solution lies in the precise stability of spinning temperature, high-precision control of metering supply, and optimized maintenance of the spinneret/cooling air field. It is recommended to start with chip quality and spinning parameters and gradually investigate to the equipment and component level.
uneven oiling agentoiling nozzle maintenanceoiling agent concentrationtemperature control stabilityyarn guide positioning