Material Analysis
4 조회수
ABAK super-tough alloy
문제 현상
Preparation of ABAK super-tough grade (Izod impact 1200J/m); optimization of SMA dosage and blending ratio.
원인 분석
For ABAK super-tough alloy, when SMA addition is 0.5% and PA6/ABS mass ratio is 90/10, the comprehensive mechanical properties are the best and the Izod notched impact strength reaches 1200J/m; processing performance is maintained; morphological structure control.
해결 방법
①SMA dosage 0.5% optimization; ②blending ratio 90/10; ③morphological structure control; ④performance testing verification; ⑤process stability.;after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
핵심 요약
ABAK super-tough alloy is a high-performance grade; precise ratio is the key; testing verifies the ultra-high toughness.;after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!