메뉴
재료 기계
인사이트
기사 동영상 문제 및 해결책
About
Chembull 소개 미디어 파트너
문의하기
언어
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
문제 및 해결책으로 돌아가기
Material Drying 4 조회수

Internal bubbles in products caused by ABS water content

문제 현상
Fine bubbles appear inside the product or in thick-wall areas; holes can be seen when cut open, often accompanied by silver streaks.
원인 분석
When the raw material is wet, water vapor turns into steam in the barrel and mixes into the melt; after filling, it is sealed inside the product to form bubbles; it is most likely to occur when the drying time is insufficient or the ambient humidity is high.
해결 방법
①Strengthen drying (80~100℃, 2~4 hours, moisture content <0.2%); ②appropriately lower the barrel temperature to reduce volatilization; ③increase back pressure to discharge gas; ④improve mold venting.
핵심 요약
For bubbles, check water content first, then check temperature and venting; the order cannot be reversed.
ABS;bubbles;moisture;drying;back pressure