Molds & Tooling 7 조회수

ABS draft angle 1.5-2°

문제 현상
ABS draft angle 1.5-2° minimum, increased for textured surfaces, demolding and deformation.
원인 분석
ABS draft angle 1.5-2° minimum for all vertical surfaces; increased for textured surfaces; smooth demolding; ejection deformation; surface quality; design specification.; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based solely on experience
해결 방법
①Draft angle 1.5-2°; ②increase for textured surfaces; ③ejection system; ④deformation monitoring; ⑤design specification.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
ABS draft angle is a design specification; textured surface compensation; ejection and surface both emphasized.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
ABS; draft angle; 1.5-2°; texture; ejection; deformation