Molds & Tooling
7 조회수
ABS draft angle design
문제 현상
[Problem phenomenon] ABS products difficult to demold and scratched, insufficient draft angle
원인 분석
Vertical wall draft angle 1.5-2° minimum, textured surfaces need larger; insufficient draft angle causes large clamping force leading to scratching and mold sticking; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based solely on experience
해결 방법
Draft angle ≥1.5-2°; increase for textured surfaces; polishing along the demolding direction; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
핵심 요약
ABS draft angle starts at 1.5-2°, textured surfaces increased; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!