Injection Molding
4 조회수
ABS burnt marks at flow end
문제 현상
ABS burnt marks at flow end, trapped gas adiabatic compression, speed and vent adjustment.
원인 분석
ABS burnt marks at flow end; air trapped gas adiabatic compression high temperature; injection speed too fast; poor venting; end converging area; recurrence after machine cleaning.; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based solely on experience
해결 방법
①Injection speed reduced in 10% steps; ②vent 0.025-0.05mm; ③end venting; ④machine cleaning; ⑤recurrence monitoring.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
Speed and venting of ABS burnt are the adjustment directions; 10% steps are a fine method; the end is the key area.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!