ABS burnt material factors
문제 현상
ABS burnt material factors, high recycled material ratio, mixed material impurities, thermal stability decline.
원인 분석
ABS burnt material factors; recycled material processed multiple times at high temperature causes molecular structure breakage and heat resistance decline; improper blending ratio; excessive mixed material impurities; color masterbatch and additives with insufficient temperature resistance decompose and blacken.
해결 방법
①Recycled material ratio control; ②mixed material impurity management; ③color masterbatch and additive temperature resistance; ④thermal stability evaluation; ⑤material inspection.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
The material factors of ABS burnt are the prevention focus; recycling and mixed material management; inspection ensures raw material quality.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!