Material Analysis
4 조회수
AEPDS low temperature toughness
문제 현상
AEPDS low temperature toughness is excellent, but lost by improper processing, low temperature application failure.
원인 분석
AEPDS combines weather resistance and low temperature toughness; EPDM glass transition temperature is low; but processing degradation or stress reduces low temperature performance; low temperature impact test; application verification.
해결 방법
①Processing protects rubber phase; ②low stress process; ③low temperature impact test; ④application verification.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
AEPDS low temperature toughness is a material advantage; processing protection is the key; testing ensures application.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!