Extrusion & Post 5 조회수

ASA co-extrusion temperature matching

문제 현상
[Problem phenomenon] ASA co-extrusion surface layer and substrate interlayer peeling, temperature setting favors one at the expense of the other
원인 분석
In ASA co-extrusion capstock process, the melt temperature and viscosity matching of surface layer and substrate (ABS/PVC/wood-plastic) determines interlayer bonding; excessive temperature difference weakens interface bonding
해결 방법
Co-extrusion each layer temperature set according to viscosity matching; ASA surface layer thin (0.5mm level) temperature takes middle value; interlayer bonding force sampling; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
핵심 요약
ASA co-extrusion looks at interlayer temperature viscosity matching, 0.5mm surface layer is classic; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
co-extrusioninterlayer bondingtemperature matchingcapstock

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다