Molds & Tooling 7 조회수

ASA nozzle cold slug prevention

문제 현상
[Problem phenomenon] ASA nozzle cold slug enters cavity forming cold slug spots
원인 분석
When nozzle temperature is lower than the melt front section, condensation at the outlet forms cold slug; when the mold has no cold slug well or insufficient cold slug well, cold material enters the cavity; during on-site investigation, verify item by item according to this mechanism, avoid blindly adjusting the machine based on experience alone
해결 방법
Nozzle temperature matched with or slightly higher than front section; mold set with sufficient cold slug wells; when mold opening interval is long, nozzle retracts to prevent drooling; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
핵심 요약
ASA cold slug spots check nozzle temperature and cold slug well capacity; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems