Incomplete crosslinking of EVA foaming
문제 현상
The product continues to shrink after demolding, and its performance does not meet the standard.
원인 분석
Insufficient decomposition of the crosslinking agent (residual amount >10%) results in insufficient crosslinking density; insufficient vulcanization temperature or time is the main cause.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
해결 방법
①Raise the vulcanization temperature to 170~180°C; ②add accelerators such as magnesium oxide; ③extend the vulcanization time; ④test the crosslinking degree for verification.; after adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
Crosslinking sufficiency determines the dimensional stability and performance of foamed products; the three elements of temperature, time, and accelerator work in synergy.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!