Material Drying
4 조회수
HDPE '2079851475616104457 parison bubbles
문제 현상
Bubbles are visible inside the parison, and weak spots appear in the container wall after '2079851475616104457.
원인 분석
Raw material moisture, feed section cooling leakage, screw and barrel wear entraining air; high regrind ratio with fine powder also brings air.
해결 방법
①Dry the raw material (pre-drying recommended for HDPE regrind); ②check for cooling water leakage in the feed section; ③check screw wear; ④increase back pressure to vent.
핵심 요약
For parison bubbles, check water first, then wear and regrind.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!