HDPE pipe surface roughness
문제 현상
The pipe outer surface shows orange peel or longitudinal brushed lines, poor gloss, rough touch.
원인 분석
Insufficient die head temperature prevents the discharge surface from fully melt-flattening; die buildup scrapes the surface; low melt temperature and poor plasticization also make the surface rough.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
해결 방법
①Increase the die head temperature to make the discharge surface smooth; ②clean the die buildup; ③appropriately increase the melt temperature to improve plasticization; ④check whether the die surface is damaged.; after adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
For surface roughness, first check the die head temperature and buildup, then check the plasticization state; die cleanliness and temperature are the first influencing factors of surface quality.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!