Molds & Tooling 3 조회수

HDPE mold temperature uniformity

문제 현상
HDPE box-type products have inconsistent shrinkage on each face and warp
원인 분석
Uneven mold cooling causes differences in crystallization and shrinkage on each face, warping the box; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
해결 방법
Water circuit homogenization design; cavity temperature difference controlled within ±5℃; strengthen the water circuits in deep cavity areas; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, to facilitate locating effective measures
핵심 요약
Box warpage is controlled by cooling uniformity; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar future problems
HDPEmold temperature uniformitywarpagewater circuit