HDPE Regrind Specks
문제 현상
HDPE product surface specks with regrind blended
원인 분석
Regrind contains contaminant particles and oxidized material; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
해결 방법
Sieve regrind to remove impurities; control the ratio; restrict use for appearance parts; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
핵심 요약
Regrind specks are controlled by sieving and ratio; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!