메뉴
재료 기계
인사이트
기사 동영상 문제 및 해결책
About
Chembull 소개 미디어 파트너
문의하기
언어
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
문제 및 해결책으로 돌아가기
Injection Molding 13 조회수

LCP Product Multi-stage Injection

문제 현상
Speed curve optimization.
원인 분석
LCP's fast-solidifying characteristic requires precise speed management; jetting and short shot risks coexist.; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based solely on experience
해결 방법
①Multi-stage injection curve; ②high-speed filling of thin-wall areas; ③deceleration at the end for venting; ④verification and optimization.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
LCP speed curves must fully exploit the fast-solidifying characteristic; the balance of high speed and venting is an art.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
LCP;multi-stage injection;speed;fast solidification;jetting;venting

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다