LDPE Film Hazy Water Marks

문제 현상
Local hazy water marks on the film surface, with uneven transparency.
원인 분석
Too low extrusion temperature gives poor plasticizing, and unmelted particles scatter light; moisture-affected resin with excessive water content also forms water marks.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
해결 방법
①Appropriately raise extrusion temperature to improve plasticizing; ②Dry the raw material to within 0.3% moisture content; ③Check screw plasticizing; ④Store sealed.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
핵심 요약
Hazy water marks are the apparent signal of plasticizing and moisture problems; these two checks can quickly locate the cause.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
LDPE; film; water mark; plasticizing; moisture exposure; temperature