LDPE Film Shrinkage Rate Fluctuation
문제 현상
The shrinkage rate of heat shrink film fluctuates between batches, and packaging effect is unstable.
원인 분석
Blow-up and haul-off process fluctuations change the orientation degree; melt index differences between raw material batches also affect shrinkage performance.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
해결 방법
①Stabilize the blow-up ratio and draw ratio; ②Control raw material batch consistency; ③Test shrinkage rate and release by batch; ④Fix process parameters.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
핵심 요약
The core indicator of shrink film is guaranteed by process stability; batch management is the key to fluctuation control.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!