Processing Machinery 4 조회수

LDPE Temperature Lower Limit

문제 현상
LDPE melt temperature set to 150℃; the film plasticizes poorly with gel particles.
원인 분석
Too low temperature gives insufficient plasticizing, and unmelted particles form gel particles; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; This mechanism has been repeatedly verified by industry literature and should be confirmed first during troubleshooting.
해결 방법
Raise melt temperature above 170℃; check heater bands; appropriate back pressure; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; Change only one variable at a time and record parameter changes to facilitate locating effective measures.
핵심 요약
The LDPE temperature lower limit ensures sufficient plasticizing; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; Incorporate this case into the defect archive as a troubleshooting reference for similar future problems.