4 조회수
LDPE Blown Film Temperature
문제 현상
In LDPE blown film, the bubble is unstable and transparency is poor.
원인 분석
Melt temperature fluctuation changes viscosity, affecting bubble stability and optical properties; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; This mechanism has been repeatedly verified by industry literature and should be confirmed first during troubleshooting.
해결 방법
Blown film temperature stably controlled at 170-210℃; uniform die temperature; temperature control inspection; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
핵심 요약
Stable blown film temperature is the prerequisite for bubble quality; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; Incorporate this case into the defect archive as a troubleshooting reference for similar future problems.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!