Processing Machinery
4 조회수
LDPE Screw Speed
문제 현상
After raising screw speed, sharkskin appears on the LDPE film.
원인 분석
Higher speed raises shear rate beyond the critical value, causing melt fracture; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; This mechanism has been repeatedly verified by industry literature and should be confirmed first during troubleshooting.
해결 방법
Control speed to keep shear below the critical value; add PPA aid to widen the window; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; Change only one variable at a time and record parameter changes to facilitate locating effective measures.
핵심 요약
Screw speed is managed by the melt fracture critical value; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; Incorporate this case into the defect archive as a troubleshooting reference for similar future problems.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!