LDPE Shrink Film
문제 현상
Shrink film shrinks unevenly and wrinkles after packaging
원인 분석
The shrink temperature and the film shrinkage rate do not match; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
해결 방법
Calibrate the shrink oven temperature curve; select grades with matching shrinkage rate; verify by packaging test; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate the effective measure
핵심 요약
Shrink film is matched according to oven temperature curve and grade; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!