Extrusion & Post
4 조회수
LLDPE casting roll temperature
문제 현상
Poor roll contact of LLDPE cast stretch film
원인 분석
Chill roll temperature or air knife condition is poor; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
해결 방법
Chill roll temperature 20-40°C; optimize air knife; clean roll surface; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
핵심 요약
Casting roll contact relies on roll temperature and air knife; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다