Injection Molding 6 조회수

MS Weld Line Management

문제 현상
MS weld lines become thicker when speed is too slow, speed and temperature balance.
원인 분석
MS weld lines become thicker when injection speed is too slow; temperature influence; gate design; venting; appearance management; strength influence.; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based solely on experience
해결 방법
①Appropriately increase speed; ②temperature management; ③gate optimization; ④venting improvement; ⑤appearance and strength balance.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
Speed management of MS weld lines is the key to appearance; balance ensures quality; design optimizes position.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
MS;weld line;speed;temperature;gate;appearance