PA12 Extrusion Wall Thickness Drift
문제 현상
【Problem phenomenon】The wall thickness of PA12 pipe drifted along the length direction, and the dimensions remained unstable after sizing
원인 분석
Unstable feeding, melt pressure fluctuation, and unsynchronized haul-off are the main causes of wall thickness drift; only adjusting the haul-off treats the symptoms but not the root cause, and the extrusion output must be confirmed stable before repairing the wall thickness; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
First stabilize feeding and melt pressure, then adjust wall thickness; haul-off speed correction is performed only after the output is stable; synchronously check vacuum sizing and cooling water flow uniformity; after adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
For wall thickness drift, first stabilize output and then adjust haul-off; with the wrong order, the more you repair, the more it deviates; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!