Molding Process
3 조회수
PA12 SLS Powder Bed Preheating Temperature
문제 현상
【Problem phenomenon】SLS printed PA12 parts had warpage deformation, incomplete sintering, or powder caking coexisting
원인 분석
Powder bed preheating must be close to the lower limit of the melting point: 170-180℃ (10-20℃ below the melting point) balances fluidity and sintering stability; too low causes insufficient sintering and weak interlayers, too high causes powder caking and dimensional drift
해결 방법
Set the powder bed temperature at 170-180℃ and calibrate uniformity by zone; monitor bed surface temperature difference with thermal imaging; fine-tune preheating in combination with laser parameters; after adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
170-180℃ powder bed is the core of the SLS window, and bed surface temperature difference must be monitored by thermal imaging; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!