문제 현상
【Problem phenomenon】SLS printed PA12 parts had large dimensional deviations, with obvious deformation at unevenly cooled locations
원인 분석
Unreasonable slicing parameters and excessively fast cooling speed are the main causes; rapid cooling after printing causes uneven crystallization shrinkage and deformation; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
Optimize slicing precision and scanning path; after printing is complete, cool naturally to room temperature before taking out the parts; after printing, anneal by holding at 100-120℃ for 2 hours to reduce dimensional deformation
핵심 요약
SLS dimensions rely on slow cooling plus annealing for stability, and the timing of part removal is also a variable; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!