Molds & Tooling
7 조회수
PA6 Sink Marks
문제 현상
Depressions on the back of rib and boss positions, obvious on the appearance surface.
원인 분석
High shrinkage + insufficient holding pressure compensation; early gate freeze-off; excessively large rib thickness ratio is a structural inducement; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
해결 방법
①Increase holding pressure and extend holding time;②control rib thickness to 50%~60% of the main wall thickness;③appropriately enlarge the gate to reduce shear rate and pressure loss;④core-pull and reduce material at thick walls to reduce shrinkage from the source;⑤strengthen local cooling for that location (add inserts or conformal water channels).
핵심 요약
PA6 sink marks = 'compensation management': holding pressure and freeze-off are the technique, rib thickness and thick walls are the root; crystalline materials shrink greatly, and compensation and structure must be emphasized equally; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!