메뉴
재료 기계
인사이트
기사 동영상 문제 및 해결책
About
Chembull 소개 미디어 파트너
문의하기
언어
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
문제 및 해결책으로 돌아가기
Material Drying 4 조회수

PA6 Regrind Problems

문제 현상
After blending regrind, strength declined and silver streaks increased, with unstable quality.
원인 분석
PA6 regrind has reduced molecular weight and absorbs moisture faster; repeated reuse causes serious degradation; crushed material contains fine powder and plasticizes unevenly; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
해결 방법
①Regrind proportion 10%~30%;②re-dry;③prohibit production with 100% regrind;④use all-new material for key stressed parts and appearance parts;⑤establish a ledger corresponding regrind batches to performance.
핵심 요약
PA6 regrind = 'proportion + drying' dual control: nylon regrind absorbs moisture fast and degrades fast; repeated reuse has high risk, and key stressed parts resolutely use new material; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence.
PA6; regrind; strength; drying; proportion

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다

ChemAI