Injection Molding 6 조회수

PA6 '2079851475616104452 uneven shrinkage

문제 현상
Large shrinkage differences in different directions of the same part, unstable dimensions.
원인 분석
Crystallization orientation anisotropy + wall thickness differences; shrinkage differs between flow/transverse directions; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; during troubleshooting, confirm item by item around key factors such as uneven shrinkage and orientation to avoid misjudgment.
해결 방법
①Optimize wall thickness uniformity to reduce differential shrinkage; ②balance holding pressure and time, taking into account both feeding and stress; ③optimize gate position and size; ④ensure uniform mold temperature; ⑤use CAE analysis to assist decision-making when necessary.
핵심 요약
PA6 uneven shrinkage='orientation and wall thickness': the anisotropy of crystalline materials is the root cause; uniform wall thickness and gate optimization are the main line; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
PA6; uneven shrinkage; orientation; wall thickness