Molds & Tooling 3 조회수

PA66 weak weld lines

문제 현상
Weld lines crack, insufficient strength.
원인 분석
Front convergence temperature insufficient, poor venting; high melting point makes the front cool faster and the convergence entanglement window shorter; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience.
해결 방법
①Raise melt temperature and mold temperature; ②open or clean vent grooves at the corresponding positions to ensure smooth gas discharge; ③increase injection speed to maintain melt front temperature and improve filling; ④adjust the gate so weld lines avoid stress-bearing areas; ⑤set overflow wells at the convergence to lead the cold front out of the cavity.
핵심 요약
PA66 weld line='convergence temperature': high-melting-point nylon fronts cool fast, so convergence temperature must be given even more fully; position planning and venting are equally important; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
PA66; weld line; venting; melt temperature; front