PA66 high-temperature retention degradation
문제 현상
Products turn yellow and brittle when production resumes after a short shutdown.
원인 분석
PA66 degrades noticeably after staying a few minutes near 290℃; shutdown without lowering temperature or emptying is the direct cause; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience.
해결 방법
①Lower temperature or empty as soon as shutdown exceeds the time limit; ②fully displace and flush with purging material before startup; ③select a matching small machine according to product weight to shorten residence time; ④monitor melt residence time to avoid exceeding limits; ⑤standardize shutdown SOP: lower temperature or empty as soon as the time limit is exceeded.
핵심 요약
PA66 residence time='minute-level management': high-temperature nylon degrades after staying a few minutes; shutdown SOP is an iron rule for quality assurance and cannot be delayed; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!