Material Drying 8 조회수

PA66 drying temperature upper limit 90℃

문제 현상
Pellets turn yellow and agglomerate after drying, injection molded products yellowish and more brittle
원인 분석
Drying temperature exceeding 90℃ causes surface oxidation yellowing of PA66 pellets and even sticking; oxidation products also become triggers for subsequent degradation and color difference, over-drying damage is likewise irreversible
해결 방법
①Hot air dehumidifying drying strictly controlled at 80-90℃; ②yellowed pellets are judged over-dried and scrapped; ③if drying is not completed after 8 hours, lower to 70-80℃ for heat preservation while waiting for production
핵심 요약
PA66 drying temperature upper limit 90℃ is stricter than PA6; what over-temperature brings is not more dryness but oxidative degradation, over-dried material can only be scrapped; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PA66; drying temperature; 90℃; oxidative yellowing; over-drying