Material Drying 4 조회수

PA66 dehumidifying drying dew point

문제 현상
PA66 dried in an ordinary oven still shows silver streaks after '2079851475616104452, measured moisture content always above 0.3%
원인 분석
PA66 has high amide group density and absorbs water fast; ordinary ovens use ambient hot air, when air humidity is high the dewatering limit can only reach about 0.3%, unable to meet the below-0.2% requirement
해결 방법
PA66 must use a dehumidifying dryer, drying air dew point below -40℃; moisture content confirmed below 0.2% by actual Karl Fischer measurement before startup; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
PA66 drying is premised on low-dew-point dehumidification, ordinary ovens cannot meet the requirement; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PA66dehumidifying dryingdew pointmoisture content

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다