PA66 mold temperature uniformity
문제 현상
PA66 same mold different cavities product dimensions differ greatly
원인 분석
Multi-cavity mold water line design unbalanced, cavity mold temperature differences cause inconsistent shrinkage, PA66 crystallization shrinkage is large and sensitive to mold temperature; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
해결 방법
Multi-cavity mold water lines designed equal-length equal-resistance; measured cavity surface temperatures controlled within ±3℃; regularly clean water lines to ensure consistent flow; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
Multi-cavity dimensional consistency relies first on water line balance, measured mold temperature is the means; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!