Processing Machinery 3 조회수

PA66 and PA6 interchange

문제 현상
Heat resistance test fails after replacing PA66 parts with PA6
원인 분석
PA66 melting point 262℃ is about 40℃ higher than PA6, and heat deflection temperature and long-term heat resistance are both superior, direct substitution fails in high-temperature conditions; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based only on experience
해결 방법
Keep PA66 for conditions above 120℃; PA6 can be considered for cost reduction of normal-temperature parts; verify according to maximum working condition before substitution; after adjustment, take continuous samples to verify the effect, confirm stability before resuming mass production
핵심 요약
PA6 and PA66 interchange is based on the temperature boundary; after confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
PA66PA6interchangeheat resistance