Material Drying
4 조회수
PA66 weld line fusion
문제 현상
PA66 two-piece set leaks in sealing test after ultrasonic welding
원인 분석
Contaminated welding surfaces or inconsistent moisture content cause poor fusion; unreasonable energy director design disperses energy; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based only on experience
해결 방법
Clean and dry welding surfaces; unify material moisture conditioning state; design energy director cross-section according to material thickness; full air-tightness inspection after welding; after adjustment, take continuous samples to verify the effect, confirm stability before resuming mass production
핵심 요약
Welding sealing is guaranteed by interface state and energy director design; after confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!