Material Drying
5 조회수
PA66 hot water hydrolysis
문제 현상
PA66 hot water pipe joints crack brittlely and leak after two years of use
원인 분석
High-temperature hot water hydrolyzes amide bonds, molecular weight continuously decreases, and the material gradually embrittles; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based only on experience
해결 방법
Switch to hydrolysis-resistant grades or PPA for long-term hot water contact; long-term hydrolysis verification is mandatory for working temperatures above 80℃; after adjustment, take continuous samples to verify the effect, confirm stability before resuming mass production
핵심 요약
Material selection for high-temperature water conditions must consider hydrolysis life; after confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!