Material Drying 4 조회수

PA6 Start-Up Pre-Drying Procedure

문제 현상
After weekend shutdown, when starting up on Monday, the first few shots show severe silver streaks and bubbles
원인 분석
During the shutdown, the PA6 in the barrel and drying hopper is exposed for a long time or insufficiently heat-preserved and re-absorbs moisture; directly using material that has not been re-dried at Monday start-up causes defects
해결 방법
Establish a start-up procedure: purge the barrel before the weekend shutdown, re-dry the material according to the standard for more than 4 hours before Monday start-up, first expel the residual material in the barrel by low-speed air shots, and confirm the extruded strand has no bubbles before production
핵심 요약
Restarting after a shutdown must re-confirm the drying state of the material, and the drying results from before the shutdown cannot be carried over; after confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence
PA6start-up procedurepre-dryingshutdown