Extrusion & Post
4 조회수
PA6 Sausage Casing Film
문제 현상
The PA6 sausage casing film has an unstable bubble and large thickness deviation during film blowing
원인 분석
PA6 melt strength is low, the film blowing bubble stability is poor, and uneven air ring cooling directly causes thickness deviation; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
Adopt the downward-blowing water-cooling process to stabilize the bubble; equalize the air ring airflow; select film blowing grade high-viscosity grades; online thickness measurement feedback adjustment for thickness deviation; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
핵심 요약
PA6 film blowing should use downward blowing with water cooling, and high-viscosity grades improve bubble stability; after confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!