Extrusion & Post 4 조회수

PA6 Material Change Purging Specification

문제 현상
After material change, the product shows color mixing, delamination and black specks, and repeated purging is still not thorough
원인 분석
PA6 viscosity is low; during purging it easily slips in layers against high-viscosity residual material, resulting in poor purging efficiency; during shutdown PA6 cools and solidifies in the barrel, and at restart the cold material mixes in and forms defects
해결 방법
①Use high-viscosity material such as HDPE or PP to flush and displace at low speed; ②Keep low speed during flushing to avoid nylon retention and isolation; ③Empty the barrel before shutdown; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
PA6 purging relies on the mechanical pushing action of high-viscosity material; low-speed flushing plus shutdown emptying is the standard procedure to avoid cross-contamination; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PA6; material change; purging; HDPE flushing; emptying

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다

ChemAI