Material Drying 4 조회수

PA6 Water Absorption Dimensional Change

문제 현상
PA6 precision parts have qualified dimensions at assembly, but the fit becomes loose after several weeks of storage
원인 분석
PA6 absorbs moisture and swells after absorbing water, and dimensions change with ambient humidity; dry-state products without conditioning treatment absorb moisture and swell in service, and precision fit dimensions drift; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based only on experience
해결 방법
After molding, precision parts are conditioned according to ISO1110 until dimensionally stable before inspection; reserve moisture expansion allowance in design; switch to low-moisture-absorption materials when dimensional stability requirements are high
핵심 요약
PA6 dimension management must consider moisture expansion, and inspection is only valid after conditioning; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
PA6 moisture expansion dimensional change conditioning

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다