Material Drying 4 조회수

PA6 Dry-State Embrittlement

문제 현상
In winter, dry PA6 cable ties and snap-fits break in large numbers during assembly
원인 분석
PA6 has poor toughness in the dry state; in winter low-humidity environments the moisture content approaches zero, notch sensitivity increases significantly, and brittle fracture occurs under assembly stress; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based only on experience
해결 방법
Condition before assembly to restore toughness; impact strength is best at moisture content 1.5-2.5%; keep inventory at a certain humidity; boil brittle-fracture batches in boiling water for 2-4 hours for rapid conditioning
핵심 요약
Dry-state embrittlement is an inherent property of PA6, and conditioning is the most effective toughness restoration means; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PA6 dry-state embrittlement conditioning toughness