Injection Molding
5 조회수
PARA Jetting Marks
문제 현상
Jetting snake marks appear in front of the gate of PARA products; improper injection point position and speed, with high-viscosity melt jetting.
원인 분석
Improper injection point position with melt rushing straight; too-fast initial injection speed with melt jetting; too-small injection point cross-sectional area with concentrated shear; PARA high-flow grades are still subject to jetting rules.
해결 방법
①Modify the injection point position to avoid straight rushing; ②Reduce the initial injection speed; ③Enlarge the injection point cross-sectional area; ④Multi-stage injection passing slowly through the gate area.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
PARA jetting marks require both gate design and speed control; injection point position is a structural factor; initial speed management is the key process.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!