문제 현상
Jetting marks and cold material spots appear on the product surface, obvious near the gate
원인 분석
Low PBT nozzle temperature produces cold material entering the cavity; an overly small gate produces jetting; low resin temperature and mold temperature aggravate front condensation; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
해결 방법
①Increase nozzle and resin temperature; ②Enlarge the gate to reduce jetting; ③Set a cold slug well to intercept the cold material at the front; after adjustment, take samples continuously to verify the effect, and resume mass production only after confirming stability
핵심 요약
PBT jetting marks are investigated along two lines: nozzle temperature and gate; the cold slug well is the interception means on the structure side; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!