문제 현상
The product develops cracks during assembly, contact with solvents, or after being left for a period of time, mostly starting from sharp corners, screw bosses, and weld lines, it is a delayed failure.
원인 분석
PC is extremely sensitive to residual internal stress; high internal stress caused by high holding pressure, uneven cooling, and large demolding ejection force induces environmental stress cracking under the action of solvents, grease, or external force; stress is the internal cause and the medium is the external cause, and neither can be absent.
해결 방법
①Reduce holding pressure and cool uniformly to reduce residual stress from the source; ②Optimize ejection to avoid ejection whitening stress; ③Structurally eliminate sharp corners and avoid excessive assembly interference; ④Avoid contact with incompatible solvents; ⑤Anneal stress-sensitive parts.
핵심 요약
The core of PC management is 'internal stress management': cracking is often a time bomb that explodes after leaving the factory; restraining the holding pressure and eliminating uneven cooling is far more effective than screening cracked parts afterwards.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!